Filter Crucibles
Material : Schott Duran Germany & Iwaki Pyrex Japan
Borosilicate glass 3.3
Idea for drying precipitates to constant mass at 110’c.I If used at higher temperatures, heating in an electric furnace is advised, and crucibles should not remove until the temperature has been reduced to about 250’C. Always take care to avoid sudden temperature changes.With intergral glass sintered disc.
Cat. No. | Nominal Capacity | Sintered Disc dam (mm) | Porosity Grade |
Overall Height (mm) |
1200.05.01 | 10 | 20 | 1 | 45 |
1200.05.02 | 10 | 20 | 2 | 45 |
1200.05.03 | 10 | 20 | 3 | 45 |
1200.05.04 | 10 | 20 | 4 | 45 |
1200.05.05 | 10 | 20 | 5 | 45 |
1201.05.01 | 30 | 30 | 1 | 53 |
1201.05.02 | 30 | 30 | 2 | 53 |
1201.05.03 | 30 | 30 | 3 | 53 |
1201.05.04 | 30 | 30 | 4 | 53 |
1201.05.05 | 30 | 30 | 5 | 53 |
1202.05.01 | 60 | 40 | 1 | 65 |
1202.05.02 | 60 | 40 | 2 | 65 |
1202.05.03 | 60 | 40 | 3 | 65 |
1202.05.04 | 60 | 40 | 4 | 65 |
1202.05.05 | 60 | 40 | 5 | 65 |
RELATED products
Related products
DURAGLAS SDN. BHD.
(200101012252 / 548008-V)
56-M, Jalan Metro Perdana Timur 11, Kepong Entrepreneur’s Park, 7th Miles,
Kepong Road, 52100 Kuala Lumpur, Malaysia
56-M, Jalan Metro Perdana Timur 11, Kepong Entrepreneur’s Park, 7th Miles,
Kepong Road, 52100 Kuala Lumpur, Malaysia
- +603-6251 7199 / +603-6252 6639 / +603-6242 7719
- +603-6258 4639
- enquiry@duraglas.com.my
© 2023 DURAGLAS SDN BHD (200101012252 / 548008-V). All Rights Reserved.